Question 254 · LDEK · Composites
In order to reduce polymerization shrinkage one can use:
1) „soft start” polymerization technique;
2) high-intensity light-curing technique;
3) bonding system dedicated to the composite;
4) thin layer of a flowable composite as a liner;
5) no thicker than 2 mm layers of conventional composite;
6) 2-5 mm thick layers of conventional composite;
7) no thicker than 6 mm layers of conventional composite.
The correct answer is:
2) high-intensity light-curing technique;
3) bonding system dedicated to the composite;
4) thin layer of a flowable composite as a liner;
5) no thicker than 2 mm layers of conventional composite;
6) 2-5 mm thick layers of conventional composite;
7) no thicker than 6 mm layers of conventional composite.
The correct answer is:
- A. 2,3,4,5.
- B. 1,3,4,5.
- C. 2,4,7.
- D. 1,3,4,6.
- E. 2,3,4,6.
Hint
Favour measures that delay the gel point, buffer stress or reduce the volume cured at once; avoid anything that speeds curing or thickens increments.
The answer, the explanation and a note on every option are available once you log in. The account is free: topic tests, a mock exam, mistake review and statistics.
More questions on Conservative dentistry
- A 23-year-old patient presents with a spontaneous pain of tooth 46 lasting for about 1 week. The pain has been much stronger since yesterday. The…
- During preparation of a cavity class II according to Black on the occlusal and mesial surface of tooth 36 in a 25-year-old patient, a carious spot…
- Which of the following concerning irrigating solutions used in endodontic treatment is true?
- Which of the following tissues are specialized connective tissues of mesodermal origin, formed from the dental papilla?
- Changes in plaque pH following a rinse with a glucose solution were first observed by Stephan. How much time the acid plaque takes to return to its…
- What is the temperature above which guttapercha becomes liquid?